Summary
Concrete contains voids that can hold air. When air moves from a susceptible base into a wet coating, it can disturb the film and contribute to bubbles or pinholes. This substrate outgassing is different from the resin’s curing reaction, and it is only one possible explanation for a visible coating defect.
Dynamic Concrete Solutions · Published 17 October 2026
For related work, see Dynamic Concrete Solutions’ epoxy and flake flooring service.
The visible face is not a solid block without spaces
A concrete surface can look dense while containing voids below it. Some voids can connect with one another and with the surface. The air in those spaces is part of the physical situation encountered by a wet layer placed above the concrete.
A simplified drawing of connected pockets helps make that arrangement visible. Real concrete does not contain the neat round chambers shown in an illustration. The exaggerated pockets are a way to show that there can be a route from below the face to the material covering it.
This is a different question from whether a coating has the desired colour or whether its surface has become dry-looking. The source of the moving air can lie in the substrate rather than in a visible feature of the decorative finish.

- Concrete can contain connected voids below the visible face.
- Air moving into a wet layer can disrupt that layer and leave an opening.
- Curing is a different process; a visible pinhole or bubble alone does not identify its cause.
A gas pathway can meet a developing film
Imagine air reaching the underside of a wet film through a connected route. For the film to remain continuous, it must respond to that disturbance as its condition changes. A small disturbance may not leave the same result as another disturbance arriving at a different stage.
The visible result could include an opening or bubble-like feature, and the drawing shows a possible sequence: a gas pathway, contact with a wet layer and a disruption in that layer.
Temperature can be relevant without being a complete diagnosis
Gas conditions can change as the surrounding material and environment change. A retrieved Sikafloor-161 technical sheet specifically describes pinholing from rising air during rising temperatures in its application context. That provides a manufacturer example of the mechanism being relevant to a concrete/coating interface.
The useful distinction is that the base is an active physical part of the situation. Observing only the air temperature or only the glossy top surface would leave other relevant conditions undescribed.
Outgassing and curing are not the same process
Curing concerns the material change of the reactive resin system. Substrate outgassing concerns gas moving from the receiving material into or through the wet layer. Both may be relevant during the same general period without being the same event.
General epoxy chemistry guidance explains the resin’s progression through changing states. Those changing states help explain why the timing of a disturbance can matter conceptually.
This separation also prevents confusion with another use of the word outgassing. Some technical documents discuss emissions measured from a product. An emissions certificate is not, by itself, a description of air escaping from concrete pores. Similar terminology can refer to different measurements and sources.
A bubble shape does not identify its origin
Air introduced during handling, moisture-related processes, contamination and layer interactions can lead to different problems that may have a superficially similar appearance. A photograph of a round feature cannot identify all of the conditions that preceded it. The outgassing explanation is one supported possibility rather than a universal label.
Likewise, a small hole is not an instruction to select a repair by its shape alone. The actual material, stage, supporting base and system evidence have to establish the relevant cause.
Dynamic Concrete Solutions’ epoxy information describes preparation and the complete floor system together. The physical lesson is that a finish receives the conditions of the material beneath it. A continuous-looking film can be affected by an invisible route from that base, while the resin’s own chemical development remains a separate part of the explanation.
A pathway matters as much as the presence of air
Imagine two enlarged voids below an invented surface. One is isolated in the sketch; the other connects to the surface through a narrow route. Both contain drawn air, but only the second illustration supplies a path from that pocket to the wet material above. The presence of a void and a route for gas movement are therefore different features.
Now consider when that route meets the coating. A wet layer, a changing layer and an already developed surface do not present identical conditions. It shows why a description of a gas disturbance needs both a source/pathway and the state of the material encountered.
This is a useful limit on the explanation. Finding that concrete contains air does not prove that outgassing caused a particular mark. The sequence and route still matter, and another source of a disturbance may remain possible. Separating those parts gives a clearer mechanism than treating every bubble-shaped feature as evidence of one familiar cause.
What should you send when asking about coating pinholes?
Give the flooring contractor a record of what you can see and when it appeared. This helps them plan an assessment; a close-up photograph alone cannot establish the cause or the right repair.
- Show the pattern: send a close-up with an indication of scale, plus a wider photograph showing where the marks occur across the floor.
- Record the timing: note when the coating was applied, when you first noticed the openings and whether their appearance has changed.
- Describe the use: explain whether the area is a garage, workshop or another space, what normally contacts the floor and when access is needed.
- Keep the floor records: provide any available product names, preparation details and installer handover instructions. Say when a detail is unknown.
Before booking a repair, ask what needs checking on site, which preparation and coating layers the proposed work includes, and when the area can return to its intended use. Agree that scope before choosing a patch or recoating method.
Call 0401 151 092 or send your project details to discuss the existing surface with Dynamic Concrete Solutions.
Explore the related Dynamic Concrete Solutions service information.
References: Sika: Sikafloor-161 product data (April 2023); WEST SYSTEM: epoxy chemistry.
Related reading: Why an epoxy floor can feel dry before it reaches full cure and Why chemical resistance is a conditional statement about a floor.
Dynamic Concrete Solutions provides epoxy and flake flooring in Brisbane. Get in touch to discuss your surface.